Page 13 - BENK YAPI - Construction Chemicals
P. 13
• After surface cleaning, the surface should be primed with Surface and Ambient Temperature
Baumix primer as a single layer in order to increase the During application, the surface and ambient temperature should
adhesion strength and balance the surface absorbency and be between +5°C and +35°C.
let it dry for 1-2 hours.
• Before applying on exposed concrete surfaces, the APPLICATION INSTRUCTIONS
surface should be primed with Baumix gross concrete Mixing ratio
primer as a single layer and left to dry for a minimum of 8 4.0 - 6.0 liters of water for 25 kg packaging
hours in order to increase the adhesion strength.
• In wet volume applications, the recommended surface Mixing Equipment
should be waterproofed with Wasserdamm elastic or • Low speed electric mixer (400 rpm)
Wasserdamm fully elastic product before laying ceramic • Special tip mixing equipment
tiles.
Mixing Time
Application Methods It should be mixed with the help of a low-speed mixer so that
• Baumix Master Kleber should be applied to the surface there are no dry powders and lumps. Mortar, 5-10 min. 1 - 2
with a notched trowel determined according to the size of minutes before the application after resting. should be mixed
the ceramic and the structural condition of the surface. again.
• Care should be taken that Baumix Master Kleber does not
form a film on the surface during application. Application Equipment
The adhesive that has formed a film on its surface should • Notched steel trowel determined according to the size of the
be scraped from the floor and should not be reused. ceramic and the structure of the floor.
• The coating material should be placed on the surface and • Rubber-tipped ceramic rammer
it should be placed on the surface with a rubber-tipped
mallet. Equipment Cleaning
• Joint filling process should be started at least 24 hours After the application, the mortar on the used equipment should
after bonding. be cleaned with water before it dries
Application should be made with Benkim Joint Filler,
Benkim Silicone Joint or Benkim Joint Filler Flex. CONSUMPTION / CONSUMPTION
• Double-sided bonding should be applied for coating The amount of consumption varies according to the condition of
applications larger than 33x33cm in outdoor applications. the application surface and the size of the coating material used.
• In exterior applications, in floor moldings up to 8 m
vertically, profile-supported 45x45 cm coating materials can PACKAGING
be adhered. Baumix Master Kleber mortar is supplied in 25 kg kraft bags.
Application Suggestions SHELF LIFE
• After mixing the product, it should be used within the pot It is 6 months when stored in its unopened original package in a
life. Products that have expired during the application dry and cool environment.
should never be used.
• Any foreign material such as lime, cement, plaster should STORAGE CONDITIONS
not be added to the prepared mortar. It should not be left in direct sunlight.
• Extra water should not be added to the mixture. The mouth of the containers should be tightly closed when not
• Application should not be made on unstable surfaces. The in use.
durability and bearing of the old surfaces should be checked
before the application process. WARNINGS
• During and after the application, the surface should be Zϯϲͬϯϴ ͗ Irritating to eyes and skin.
protected from air currents and contact with water. Zϰϯ͗ May cause sensitization and sensitization by skin contact.
must be prevented. ^Ϯ ͗ Keep out of reach of children.
• It should not be applied on surfaces where there is a ^ϮϰͬϮϱ ͗Avoid contact with eyes and skin.
danger of frost within 24 hours, frozen or melting ice. ^Ϯϲ ͗ In case of contact with eyes, rinse immediately with
• Care should be taken not to expose the material to direct plenty of water and seek medical advice.
sunlight in hot weather and the mixture should be made ^Ϯϴ ͗ In case of skin contact, wash immediately with plenty of
with cold water. water.
• Application should not be made on extremely windy or ^ϯϳ ͗ Appropriate protective gloves should be used.
hot surfaces exposed to direct sun.
• Application should not be made in rainy weather, the
application surface should be protected from rain for 24
hours.
13